DOI | Trouver le DOI : https://doi.org/10.1179/136404604225014864 |
---|
Auteur | Rechercher : Jiang, Jiaren1; Rechercher : Liu, Xing Yang1 |
---|
Affiliation | - Conseil national de recherches du Canada. Institut des matériaux industriels du CNRC
|
---|
Format | Texte, Article |
---|
Sujet | solid ceramic mould casting; burning-out; gelling of ethyl silicate binder; casting accuracy; precision casting |
---|
Résumé | Burning-out is an important step in mould fabrication for the ceramic mould casting process to remove alcohol in the gelled ethyl silicate binder. It affects both the accuracy and stability of the ceramic mould dimensions. In this paper, results are described for length changes of ceramic mould specimens during the burning-out process after alcohol immersion or drying in air for various lengths of time. It is shown that preventing rapid evaporation/removal of alcohol from the ceramic mould specimen before burning-out by immersing the specimen in alcohol generally produces less overall length change compared to leaving the specimen to dry in air. The immersion time for the specimen in alcohol or drying in air before burning-out has a significant effect on the overall length changes in the specimen and on the characteristics of the burning-out curves. Under the conditions investigated, immersing in alcohol for 5–10 h followed by burning-out produced near zero overall length change in the specimen. |
---|
Date de publication | 2004-02-01 |
---|
Dans | |
---|
Langue | anglais |
---|
Publications évaluées par des pairs | Oui |
---|
Numéro NPARC | 21272501 |
---|
Exporter la notice | Exporter en format RIS |
---|
Signaler une correction | Signaler une correction (s'ouvre dans un nouvel onglet) |
---|
Identificateur de l’enregistrement | 3f85c72a-27fc-4d89-b476-dbc1c139c677 |
---|
Enregistrement créé | 2014-12-01 |
---|
Enregistrement modifié | 2020-04-17 |
---|