Auteur | Rechercher : Tramblay, S.; Rechercher : Champagne, B.1; Rechercher : Angers, R. |
---|
Affiliation | - Conseil national de recherches du Canada. Institut des matériaux industriels du CNRC
|
---|
Format | Texte, Rapport technique |
---|
Résumé | A method to produce dense WC-Co spheroidal particles was developed. The method consists in agglomerating mixtures of WC and Co powders with a paraffin binder in a tiled rotating cylinder. After a presintering step, the particles are cold isostatically pressed and sintered under vacuum at 1450oC. The resulting particles are fully dense. Particles containing 5, 10 and 15 wt % Co were fabricated. The agglomeration mechanisms and the characteristics of the WC-Co particles are discussed. |
---|
Date de publication | 1984 |
---|
Maison d’édition | National Research Council of Canada. Industrial Materials Research Institute |
---|
Série | |
---|
Langue | anglais |
---|
Publications évaluées par des pairs | Non |
---|
Numéro du CNRC | NRCC 23799 |
---|
Numéro NPARC | 23004340 |
---|
Exporter la notice | Exporter en format RIS |
---|
Signaler une correction | Signaler une correction (s'ouvre dans un nouvel onglet) |
---|
Identificateur de l’enregistrement | c9a5d00b-0d21-444d-878a-d20f243e543f |
---|
Enregistrement créé | 2018-10-24 |
---|
Enregistrement modifié | 2023-01-13 |
---|